Thermal shock is defined by the rate of temperature change at the sample, not by the set points. Move a part from −40 °C to +125 °C in ten seconds and the surface is in compression while the core is still cold; move it in two minutes and the gradient is mild.

That is why the same profile on two machines produces two different results, and why the transfer time belongs in the test report next to the temperatures.

What each method is good at

PropertyTwo-zone air chamberLiquid bath (perfluorocarbon or oil)
Transfer time5 s to 15 s typical2 s to 5 s
Heat transfer coefficientLow, airHigh, liquid
Sample stressModerate, driven by air movementSevere, driven by contact
Best forAssemblies, populated boards, productsComponents, seals, small parts
Contamination riskNoneLiquid residue must be removed
ThroughputModerate, one basketHigh, two baths running continuously
Typical range−70 °C to +180 °C−65 °C to +200 °C

A two-zone chamber is a compromise that keeps the product clean; a liquid bath is a stress test that finds cracks a chamber would miss, at the cost of cleaning and of not being usable on porous parts.

Transfer time, measured not assumed

The transfer time that matters is the time for the sample surface to reach within a few kelvin of the new setpoint, not the time for the basket to move. A basket that moves in 8 s can take 90 s to bring a 200 g aluminium block to temperature.

  • Tape a thermocouple to the sample. Log the curve for one cycle before running the batch.
  • Check the dwell. The dwell must start when the sample is at temperature, not when the chamber is.
  • Count the cycles the same way every time. One cycle is one hot dwell plus one cold dwell.
  • Note the recovery. A chamber that takes 15 min to recover between cycles is running a slower test than its programme claims.

Failure signatures

Solder joint cracks appear after a few hundred cycles in a liquid bath and after a thousand in a chamber: the mechanism is the same, the rate is not. Seal failures show as a slow leak that only appears after the sample returns to room temperature, which is why the leak check belongs at the end of the run and not in the middle.

Our thermal shock systems are quoted with a measured transfer curve rather than a nominal one, and the technical notes give the sample masses that each size can move inside the specified time.

Standards referenced: IEC 60068-2-14 test Na and Nb, IEC 60068-2-14 clause 8 (transfer time), JESD22-A104 for the component-level equivalent.

Cost per cycle, and why it matters more than the chamber price

A two-zone chamber at 5 cycles per hour produces 40 cycles in an 8 h shift; a liquid bath at 12 cycles per hour produces 96. For a 500 cycle qualification that is 13 shifts against 5, and the labour cost difference is larger than the equipment price difference.

  • Count the cycles you actually need before choosing the method.
  • Add the cleaning time for liquid methods, typically 10 min per batch.
  • Check whether the product can be immersed at all before quoting the faster option.

Contact Us

Contact: Eason Wang

Phone: +86-13751010017

Tel: +86-755-33168386

Add: 1F Junfeng Building, Gongle, Xixiang, Baoan District, Shenzhen, Guangdong, China

close
Scan the qr codeClose
the qr code